Weld Defects
Welding Positions
Electrode Knowledge
Pass or Fail?
Shop Troubleshooting
100

What weld defect appears as a groove along the toe of a weld?

Undercut

100

What welding position is called the flat position?

1F or 1G

100

What does the E at the beginning of E7018 mean?

Electrode

100

You see several small holes across the surface of a weld. What defect are you looking at?

Porosity

100

What happens to the arc if an SMAW electrode is held too far away from the workpiece?

The arc becomes too long and unstable.

200

What defect occurs when weld metal rolls onto the base metal without properly fusing to it?

Overlap

200

What position are you welding when making a horizontal fillet weld on a T-joint?

2F

200

In E7018, what do the first two digits — 70 — represent?

70,000 psi minimum tensile strength

200

A fillet weld has one leg much larger than the other. What should the welder improve?

Weld size/profile and consistency

200

What is one likely result of traveling too slowly while welding?

An excessively wide or large weld bead, excessive buildup, or possible overlap.

300

What defect appears as small holes or cavities caused by trapped gas in the weld?

Porosity

300

What does the letter F mean in 2F?

Fillet weld

300

What does the 1 in E7018 indicate?

The electrode can be used in all welding positions.

300

The weld bead is straight and consistent, but there is a visible groove running along one toe. What defect should be recorded?

Undercut

300

What can happen if your travel speed is too fast?

A narrow bead, poor fusion, insufficient weld size, or undercut.

400

Name one common cause of slag inclusion.

Failure to remove slag between passes, improper electrode angle, or incorrect welding technique.

400

What does the letter G mean in 3G?

Groove weld

400

Which electrode is known as a low-hydrogen electrode: E6010 or E7018?

E7018

400

Before inspecting a finished weld visually, what should normally be removed from the weld surface?

Slag, spatter, and anything preventing proper visual inspection.

400

Your electrode keeps sticking to the workpiece when you try to strike an arc. What machine setting might be too low?

Amperage

500

A weld looks good on the surface but the weld metal did not properly join to the base metal. What defect may be present?

Lack of fusion

500

In what position is a 4G groove weld performed?

Overhead

500

Why should E7018 electrodes be protected from excessive moisture?

Moisture can increase hydrogen in the weld and contribute to hydrogen cracking or weld defects.

500

Name four things you could evaluate during a visual inspection of a fillet weld.

Examples include weld size, profile, uniformity, undercut, overlap, cracks, porosity, fusion, crater condition, and overall workmanship.

500

A welder keeps getting slag trapped between multiple weld passes. What should they change?

Completely remove slag and clean each pass before depositing the next weld.