Preferred current for GTAW welding mild steel
DCEN
Recommended post flow time for welding at 200amps
20 secs
1 sec for every 10 amps
Yellow band on one end of tungsten
1% thoriated
This component ensures electrical contact between the torch body and the collet
Collet body
This metal requires back purging using GTAW
Power source used for GTAW
Constant Current
L/min and CFH
Red bad on one end of tungsten
2% thoriated
These are known as
Back caps
deoxidized filler rods are used for mild steel
control porosity
Type of current that promotes greater control over heat input
Pulsed
Preferred shielding gas for GTAW heavier gauge aluminum
Helium
Brown band on one end of tungsten
Zirconium
Component known as
Collet or Electrode Collet
Rule of thumb for estimating GTAW stickout
1 to 2 electrode diameters
Which half cycle is reduced using GTAW process on AC
DCEP
Shielding gas preferred for light gauge material
Argon
Blue band on one end of tungsten
EWTh-3
Pure tungsten and thorium
Component known as
Collet body
Amperage limit for air cooled GTAW torches
150A
DCEN with HF is used to provide
Non touch arc start
Excessive gas flow causes what GTAW defect typically and what is the correct flow rate for GTAW
Undercut
15 to 25 CFH
Most commonly used electrode for welding magnesium alloys
EWZr
Component know as
Gas lens
Maximum water pressure that should be used with water-cooled GTAW torches
245 to 280 kpa ( 35 to 40 psi)