AWS D1.1
API 1104
ASME SEC. 9
TEST DAY
CARBON CONTENT
100

What is the MAX cover pass height on a D1.1?

1/8"

100

What does API stand for?

American Petroleum Institute 

100

What does ASME stand for?

American Society Mechanical Engineers 

100

What is the first hold point for a test day?

Fit-Up

100

Whats the carbon content of Low Carbon steel?

.1-.3%

200

How wide is your D1.1 side bend sample?

3/8"

200

What industry is the API code most prevalent? 

Oil and Gas

200

What Section applies to welders in the ASME code?

Section 9

200

What is the second hold point of test day?

Root pass check

200

Whats the carbon content of Medium Carbon steel?

.3-.5%

300

What is the root gap size for the D1.1?

1/4"

300

Name at least 2 welding rods are used on a API 1104 weld?

6010, 7010, 8010

300

What is the name of section 9?

Welding and brazing of pressure vessels.

300

What is the 3rd hold point for combo pipe tests?

After TIG hot pass before taking down pipe for booth switch. 

300

Whats the carbon content of High Carbon steel?

.5-.9%

400

What is the max incline degree aloud on a 3G or 4G test.

+ or - 10 Degrees 

400

Is API considered High, Medium, or Low pressure piping?

High Pressure

400

What is the max reinforcement of the root pass for a ASME?

1/8" but a 1/16" is ideal 

400

What are 3 things that could fail you other then your welds?

No safety glasses, rods on the ground, going into other booths, not getting inspector for hold points, profanity, attitude, leaving the premises etc.  

400

Whats the carbon content of tool steel?

1.4%

500

What is the max length of a single discontinuity on a D1.1 bend sample?

1/8"

500

Is the API test in 5G or 6G?

6G

500

If you pass a 6G ASME does that qualify you for a 3G unlimited 7018 D1.1?

yes 

500

Why should you stay within the heat range on your test piece?

So you don't exceed the HAZ range to cause embrittlement. And so your weld doesn't drip on you.  

500

What metal has a carbon content of 2-4% 

Cast Iron