W
E
L
D
S
100

Electric current is measured in this scale

What is Amperage

100

How hot is the puddle in the SMAW process

Hot- up to 10 0000 F

100

the maximum electrical potential difference (Voltage) between the terminals of a device when there is no load

What is open circuit voltage

100

Which electrode diameters are better with vertical or overhead positions

What are smaller diameter electrodes

100

Cracking that occurs shortly after the weld metal has been deposited and is just beginning to solidify is called

What is hot-cracking

200

This type of current may produce arc blow

What is Direct Current

200

Electrodes range is sizes from 1/16" to

....To 5/16

200

SMAW welding machines are this type of power source

What is Constant Current

200

Which stainless electrode is suitable for welding low-carbon steel to stainless steel

What is E309-15

200

This is a crack across the face of the weld

What is a Transverse crack

300

These methods can be used by the welder to spread heat evenly while welding 

What is Back-stepping, intermittent weld sequencing and Alternate back-stepping

300

This is the most common welding electrode length

What is 14"

300

What is the advantage of DCEN over DCEP in the SMAW process

DCEP ability to produce shallower penetration and faster deposition rates

300

These three electrodes are suitable for welding cast iron

ECI 

ESt

ENi

300

A crack that is length ways along the weld, sometimes into the base metal

What is a longitudinal crack

400

List five factors help with metal transfer across the arc?

Gravity,  Gas Expansion, Electromagnetic Force,

Electromotive force, Surface tention

400

EIectrodes are classified according to deposition characteristics.

What are the F catagories

400

This device changes AC to DC

What is a diode rectifier

400

These electrodes need to be stored in an electrode oven

Low-Hydrogen

Hard-facing

Special Alloys(eg.stainless steel)

400

The Mixing of the base metal and hard-facing material

What is dilution

500

Which ingredient in the flux of welding electrodes is responsible for the inverted cup type characteristics on the coating during welding

What is Cellulose

500

What organization developed the most general classification for welding electrodes

What is ASME

500

When you lengthen the arc this happens to the voltage and amperage?

Volts go up

Amperage goes down

500

This is the proper number and letter abbreviation when a pipe is in a 45 0 incline and fixed position

What is 6G

500

There are three methods of mechanical distortion control

What are Pre-bending, Clamping, Pre-spacing

M
e
n
u