Strike the Iron while the Iron is Hot
With the welding machine on but no arc has been struck it will produce this kind of voltage
What is open circuit voltage
Sanding disks or belts have a numerical system for different grades of abrasives. The higher the number rating means...
The higher the number means the finer the grit or cut of the abrasive
Power sources used for the GTAW process
What are Constant Current power sources
When using the SMAW process an increase in arc length will cause this
What is an increase in Arc Voltage and a decrease in amperage
Once an Apple has fallen, you will see it on the ground nearby the Tree from which it dropped.
The Apple doesn't fall far from the Tree
To reduce arc blow the welder can do this
What is keeping the arc as short as possible
The height to base ratio for correct ladder placement
What is 4 : 1
The Preferred filler wire for welding on mild steel base metal
What is ER-70S-2
This TOXIC gas is created when welding with E309L
What is Hexavalent Chromium
Rome is a special area that requires the use of Boost to get around. See those Romans over there? Use Boost to see if you can keep up with them!
When in Rome do as the Romans do
Besides making the shielding gas the coating on E7018 also helps with this...
What is helping with arc stability
The load lifting capacity of forklifts depends on the spacing of the forks, the ground conditions and...
What is the height and tilt of the mast
GTAW on Ferrous metals uses this polarity to concentrate heat in the base material
What is DCEN
Dilution in hard-surface weld deposits can be caused by this...
What is mixing of base and filler metals
Measuring distances in Minecraft can be tedious, but a few simple guidelines can prevent you from making mistakes.
Measure twice Cut once
How many times does the current change direction per second when using a transformer type welding machine
What is 120 times per second
The preferred spread angle for lifting with 2 slings
What is 60 Degrees
Protecting the backside of stainless steel welding is known as this
What is back purging
Done to decrease internal stresses in the weldment
What is pre and post heat treatment
Distant grass will always have a greener hue. You can fine-tune the appearance of distant grass in Settings > Graphics.
The grass is always greener on the other side
These are the 5 essentials variables of SMAW
What is electrode size, Current, Arc length, Travel speed, Electrode angle of travel
Care must be taken to ensure that no power is lost to this tool or it will lose adhesion at the base
What is a mag-drill
The Weld discontinuity of this particular type of inclusion is found only when using the GTAW process
What is Tungsten inclusion
By using E7028 that have been left out for more than 2 hours the welder is risking this happening to the weldment
What is Hydrogen cracking