100

An intentional or unintentional interruption in the physical structure or configuration of a part

discontinuity 

100

A set of instructions or standards invoked by a specific customer to govern the results or performance of a specific set of tasks or products

Specification 

100

In arc or gas fusion welding, a cavity in the weld bead surface, typically occurring when the heat source is removed and insufficient filler metal is available to fill the cavity.


Crater / crater crack

100

The central cavity formed during solidification of metal, especially ingots, by thermal contraction

Shrink pipe / shrinkage

100

This is the state nut

hazelnut (filbert)

200

An NDT response that requires interpretation to determine its relevance

indication 

200

Document to control and govern practices in an industry or application, applied on a national or international basis and usually produced by consensus

Standard 

200

A discontinuity in metal resulting from the creation or coalescence of gas. Very small pores are called pinholes.


porosity

200

Discontinuity caused by two streams of semi-molten metal coming together inside a mold but failing to fuse.

Cold Shut 

200

This river that runs predominantly north was discovered in 1792

Willamette 

300

An NDT indication that is interpreted to be caused by a condition other than a discontinuity or imperfection

false indication


300

An instruction that is specific to how to tests a certain part. Usually outlines specific step by step details for a specific inspection.

Technique

300

Propagating discontinuities caused by stresses such as heat treating or grinding. Difficult to detect unaided because of fineness of line and pattern

crack cracking (crack kills)

300

In metal, external or internal rupture caused by improper forming

Forging Burst 

300

This is the deepest river gorge in north america

Hells Canyon (8000')

400

An NDT indication that is caused by a condition or in a location that does not affect the usability or integrity of the object

non relevant

400

Society that publishes documents that relate to the qualification and certification of personnel

ASNT

400

Cracking that is perpendicular to the long axis of the weld

Transverse 

400

A discontinuity caused by escaping gas, usually in a casting.




Blow Hole (John)

400

This rock is the third largest ocean monolith in the world and is off cannon beach

Haystack rock (235')

500

Discontinuities that are associated with the melting and solidification of the ingot before it is formed into slabs, blooms, and billets.

Inherent

500

This code was born out of necessity and to implement safe practice regarding manufacture and inspection. One of the first.   

ASME Boiler and Pressure Vessel Code

500
A groove cut at the toe of the weld, most often on the upper toe of a fillet weld. 

Undercut

500

A foreign substance within the ingot or cast part. 

Inclusion 

500