The complete curing of a composite resin can be determined by

keeping a test sample of the resin used


100

The fabric layer in the vacuum bagging process that determines the amount of resin removed from the laminate component is known as the

bleeder/breather

100

Moisture, mildew, chemicals, and acids have no effect on

What is glass fabric?

100

The loose fibers that are mixed into a matrix for added strength is known as

flox

100

The preferred way to cut curves into transparent plastics is to use a

band saw


200

What is the role of the matrix component in the composite material?


The matrix supports the fibers and bonds them together

200

An NDI method where very high frequency sound waves are induced into a composite structure to detect the presence of delaminations, voids, or inconsistencies is known as

ultrasonic testing


200

What is the recommended fastener for a composite panel that must be removed periodically for maintenance?

Screw and nutplate

200

The preferred way to cut closed cell foam core material is a/an

hot wire cutter

200

The length of time that a catalyzed resin will remain in a workable state is called the

pot life


300

The fibrous material that is used in advanced composite structures that has concerns with steel fasteners because of galvanic corrosion is

Carbon fiber

300

Styrofoam products used in aircraft composite construction are

closed cell products

300

A matrix has a pot life of 30 minutes. This means that the matrix will

cure in 30 minutes

300

To prevent premature curing, all prepreg materials must be stored

in a refrigerated environment under 0 degrees F


300

A potted compound repair on honeycomb can usually be made on damages less than

.5 inch in diameter


400

Microballoons used in composite structures

are used with matrix to fill minor voids

400

During NDI, it is found that several layers of fiber have separated from each other. This damage would be classified as

delamination

400

Fiberglass laminate damage not exceeding the first layer or ply can be repaired by  

filling with a putty consisting of a compatible resin and clean, short glass fibers

400

The coefficient of expansion of most plastic enclosure materials is

greater than both steel and aluminum

400

The part of a replacement honeycomb core that must line up with the adjacent original is the

ribbon direction


500

How would a technician test a composite structure to determine if it is electrically bonded?

Use an ohmmeter to check resistance between the composite and surrounding aircraft structure

500

How do composite materials dissipate the electrical currents that result from a lightning strike?

A conductive mesh or layer is installed in the surface ply of the composite

500

Structural properties of composite laminates such as stiffness, dimensional stability, and strength depend on

the stacking sequence and orientation of the plies


500

When repairing large, flat surfaces with polyester resins, warping of the surface is likely to occur. One method of reducing the amount of warpage is to

use short strips of fiberglass in the bonded repair

500

One method of inspecting a laminated fiberglass structure that has been subjected to damage is to

strip the damaged area of all paint and shine a strong light through the structure