GMAW 1
GMAW 2
GMAW 3
GMAW 4
GMAW 5
100

AWS restricts the level of sulfur and ____ in GMAW electrodes due to undesirable welds and cracking. 

  • Copper
  • Silicon
  • Zirconium
  • Phosphorus

Phosphorus

100

Welding too ____ a travel speed produces a _____ bead sitting on top of the base metal.

  • Fast, wide
  • Slow, convex
  • Fast, narrow
  • Slow, narrow

Fast, narrow

100

Electrode diameter will limit _____.

  • Voltage
  • CTWD
  • Amperage
  • Travel speed

Amperage

100

To provide a proper seal, double-seat seal cylinder valves must be opened ___.

  • 1/4 turn
  • 1/2 turn
  • 1 turn
  • All the way

All the way

100

The percentage of time in a 10 minute period that a power source can be operated continuously at the rated amperage before over heating is ____.

  • Open amperage
  • Output range
  • Input range
  • Duty cycle

Duty cycle

200

Higher silicon and ___ deoxidizer level enhances toe wetting and finished weld bead appearance.

  • Vanadium
  • Molybdenum
  • Manganese

Manganese

200

Welding with GMAW utilizes the polarity ____ .

  • CFH
  • DCEN
  • AC
  • DCEP

DCEP

200

Cylinders are under extreme pressure at approximately ___ psi. 

  • 4500
  • 2500
  • 3500
  • 1500


2500

200

___ mode of metal transfer typically begins at 125 amps and uses a continuously fed solid-or metal-cored wire electrode depositing in a combination of short circuits and gravity assisted large drops.

  • Short circuit
  • Axial spray
  • Globular transfer
  • None of the above

Globular transfer 

200

When welding make sure the work cable is connected ___ to the part being welded.

  • Parallel
  • As close
  • At a right angle
  • Perpendicular 

As close

300

Argon and ___ are classified as inert shielding gases.

  • Hydrogen
  • Nitrogen
  • Carbon dioxide
  • Helium

Helium

300

___ mode of metal transfer is capable of root pass work on pipe and has all weld position capability. 

  • Axial spray
  • Globular transfer
  • None of the above
  • Short circuit 

Short circuit

300

To provide corrosion resistance on weathered steel when welding requires the electrode to contain 1% ___.

  • Chromium
  • Aluminum
  • Manganese
  • Nickel

Nickel

300

Load range and ____ are the two basic components of fatigue on a weld.

  • Toughness
  • Tensile strength
  • Ductility
  • Load cycle

Load cycle

300

For Gas Shielded Arc Welding the AWS Specification for Carbon Steel Filler Metals is ___.

  • A5.00
  • A5.28
  • A5.50
  • A5.18

A5.18

400

Classification of electrode that contains the highest levels of silicon is ____ 

  • ER70S-4
  • ER70S-7
  • ER70S-3
  • ER70S-6

ER70S-6

400

Larger diameter electrodes usually ___ .

  • Cost less
  • Feed better
  • Carry more current
  • All of the above

All of the above

400

___ mode of metal transfer creates an excellent finish weld bead appearance and has the highest operator appeal.

  • Globular transfer
  • Axial spray
  • Short circuit
  • None of the above

Axial spray

400

Welding operation inspection includes which of the following ____.

  • Joint alignment
  • Burn through
  • Travel speed
  • Surface condition

Travel speed

500

When trouble shooting a GMAW system categorize the problem into one of the three groups: wire delivery, gas delivery or ___.

  • Travel speed
  • Electrical
  • Cold feed
  • Electrode extension

Electrical

500

_____ electrode extension increases the resistance to the flow of current in the electrode and the current in the arc is _____.

  • Decreasing, decreased
  • Increasing, increased
  • Increasing, decreased




Increasing, decreased

500

A common problem with GMAW-S is ___. 

  • Undercut
  • Excessive face reinforcement
  • Porosity
  • Cold lap

Cold Lap

500

A deep and broad penetration profile characterizes the use of ___ as a shielding gas in the GMAW process.

  • Nitrogen
  • Carbon dioxide
  • Hydrogen
  • Argon

Carbon Dioxide