Definitions
Suitable for service
Repair and Alteration
Dismantling and Reconstruction
Examination and testing
100

Repair

Work necessary to maintain or restore a tank to a condition suitable for safe operations.

100

What are some common causes for bottom failure.

A) internal pitting 

B) corrosion of welds

C) weld joint cracking history

D) the lack of an annular plate ring when required.

E) underside corrosion (normally in the form of pitting)

100

Nozzles for hot taps are limited to what maximum diameter.

4 inch NPS

100

The tank shall be _____ and _______  prior to commencement of dismantling.  

Cleaned, Gas-freed

100

NDE shall be preformed in accordance with? (code and section)

API 650 section 8

200

As-built standard

The standard (such as API standard or UL Standard) used for the construction of the tank component in question. 

200

When the results of a tank inspection show that a change has occurred from the original physical condition of that tank, an _______ shall be made to determine its ________ for continued use.

Evaluation, Suitability 

200

Welded-on patch plates over existing patches are not allowed in the _______________.

Critical zone.

200

When should piece markings be done.

Prior to dismantling for ready identification and placement when tank is reconstructed 

200

Cavities resulting from gouging or grinding operations to remove weld defects shall be examined by the 

magnetic particle or liquid penetrant method

300

Break-over point 

The area on a tank bottom where settlement begins.

300

Tank roof evaluation- roof plates corroded to an average thickness of less than___ in any _____ area or roof plates with any holes through the roof plate shell be repaired or replaced.

0.09in, 100in sq 

300

What is the minimum dimension for a replacement shell plate 

12 inches or 12 times the thickness of the replacement plate, whichever is greater.

300

when cutting alongside of remaining welds during dismantling of a tank, what is the minimum distance from the remaining weld that must be maintained.

2 inches

300

bottom plate repairs can be tested using what methods.

magnetic particle, vacuum box and solution, or tracer gas and detector. 

400

Candidate Tank

The tank(s) for which the corrosion rates are not known.

400

What are the principal causes of foundation failure. 

Settlement, erosion, cracking, and distortion of concrete. 

400

the maximum and minimum repair plate dimensions using lap-welded patch plates.

48 inches by 72 inches, with a minimum of 4 inches.

400

what is the minimum number of matching center punch marks are required on shell plate to facilitate alignment for reconstruction.

two sets

400

When is a Hydrostatic testing, held for 24 hours shall be performed 

on a reconstructed tank, any tank that has undergone major repairs or major alterations, a tank where an engineering evaluation indicates the need for a hydrostatic test due to an increase in the severity of service.

500

Control tank

The tank(s) for which the corrosion rates and service history are known and documented.

500

Widely scattered pitting may be ignored if?

A) no pit depth results in the remaining shell thickness being less than 1/2 the minimum acceptable tank shell thickness exclusive of corrosion allowance

B) The sum of their dimensions along any vertical line does not exceed 2in. in  an 8in length.

500

when repairing a tank floor a patch-plate may be smaller than 12 inches if it meets what criteria 

It is equal to or exceeds 6 inches in diameter; it does not overlap a bottom seam; it is not placed fully or partially over an existing patch; and it extends beyond the corroded bottom area, if any, by at least 2 inches.  

500

What is the tank Radii tolerance for a tank that is 200ft in diameter.

+ or - 1 inch

500

Stress in a repaired area shall not exceed _____ lbf/in sq

7000