Metal G
Carpet Munchers
Metal is hard
Book nerd
Good from a far but far from good
100

Wrought iron was once a very common material for what?

Structal use    PG6

100

BCC stands for what   FIG 7

Body-centered cubik

PG 25

100

In pure iron at temps above 96°C / 1670°F the atoms are arranged how 

In a fcc pattern or lattuce 

PG 25

100

Do NOT Stack or store stainless steel with 


Carbon steel

PG 64

100

What are two main considerations when welding ferritc stainless steel

Minimizing grain growth 

Per venting sensitization

PG 57

200

What is the true aging temp of alloy 6063

175°C or 347°F

PG 75

200

Two major groups of low alloy steels are 

Low-alloy, high strength low-alloy 

PG 48

200

A20/A20M are standard specifications for what

Steel plates for pressure vessel 

PG 12

200

Most aluminum is used in the form of an alloy the alloys fall into 2 broad groups


Wrought alloys and casting alloys

Pg72

200

What is longitudinally 

Running length wise or pertaining to length 

PG 18

300

At cooling rates that are between slow cooling and quenching in water various amount of what form

Ferrlte peartree martensite 

PG 28

300

Grain is 

A crystal structure with a research pattern of atoms extending across it in a polycrystalle material 

PG18

300

Nickle added in amounts of 1% improves what


Impact property at modest temps

PG 49

300

Each steel in the system is typically given a 4 digit numerical code that relates to it composition what do the digits indicate?

List all in order 

First: The major class 

Second: The sub class carbon content 

Thrid: and forth the carbon content in hundredths of a persent

Pg11

300

What are the 4 types of distortion 

Bending, buckling, angular, shrinkage 

PG 46

400

What alloying elements help with atmospheric corrosion resistance 

LIST ALL OF THEM or NO points

Copper, chromium, nickle, tantalum 

PG 30

400

The time required for sensitisation to occur depends on the carbon content of the stainless steel 

Peak temp during the welding time at peak temp 

PG 55

400

Duplex stainless steel microstructure is a mixture of austenitic and forritc grains what is the true ideal mixture

50/50 

PG 60

400

At 938°C / 1688°F there will be no evidence of what In carbon steel

Carbon 

PG 26

400

The specifications for most solid wires and metal core wires limit both sulphur and phosphorus to what 

0.03% 

PG 57

500

Sand casting has an ultimate MPA of what

207

PG 69

500

I'm excessive amounts of sulphur may lead to 

Lot shortness

Pg48

500

Aluminum alloy AA-6061 conducts heat 43% faster then.........................?


AA-5083 

pg 64

500

In 300 series austenitic stainless steels sulphur content is melted to

0.045%

PG 57

500

Surface damage such as ATC strikes and scratches may also act as 

Corrosion initiation sites

PG 65